Grade : | SUS317L耐腐蝕鋼片/板和帶材 | |||||||
Number: | X2CrNiMo18-15-4 | |||||||
Classification: | 奧氏體不銹鋼-特殊等級 | |||||||
Density: | 8 g/cm 3 | |||||||
Standard: | EN 10088-2:2005不銹鋼。通用耐腐蝕鋼片/板和帶材交貨技術(shù)條件 | |||||||
EN 10088-3:2005不銹鋼。一般用途耐腐蝕鋼的半成品、棒材、線材、型材和光亮產(chǎn)品的交貨技術(shù)條件 | ||||||||
EN 10028-7:2007壓力用鋼制扁平產(chǎn)品。不銹鋼 | ||||||||
EN 10217-7:2005壓力用焊接鋼管。不銹鋼管 | ||||||||
EN 10253-3:2008對焊管件。無特殊檢驗要求的鍛造奧氏體和奧氏體-鐵素體(雙相)不銹鋼 | ||||||||
EN 10253-4:2008對焊管件。有特殊檢驗要求的鍛制奧氏體和奧氏體-鐵素體(雙相)不銹鋼 | ||||||||
EN 10088-1:2005不銹鋼。不銹鋼清單 | ||||||||
EN 10088-5:2009不銹鋼。建筑用耐腐蝕鋼棒材、棒材、線材、型材和光亮產(chǎn)品的交貨技術(shù)條件 | ||||||||
EN 10088-4:2009不銹鋼。建筑用耐腐蝕鋼片/板和帶材交貨技術(shù)條件 | ||||||||
Equivalent grades: | ||||||||
Chemical combbbbbbbb % of steel X2CrNiMo18-15-4 (SUS317L ): EN 10088-2-2005 | ||||||||
特定的硫含量范圍可以改善特定的財產(chǎn)。對于可加工性,建議并允許將硫含量控制在0.015%至0.030%之間。對于可焊性,建議并允許將硫含量控制在0.008%至0.030%之間。對于可極化性,建議將硫含量控制在最大0.015%。 | ||||||||
未經(jīng)買方同意,不得故意將本表中未列出的元素添加到鋼材中,除非對鑄件進行精加工。 | ||||||||
C | Si | Mn | Ni | P | S | Cr | Mo | N |
max 0.03 | max 1 | max 2 | 13 - 16 | max 0.045 | max 0.015 | 17.5 - 19.5 | 3月4日 | max 0.11 |
Mechanical properties of steel X2CrNiMo18-15-4 (SUS317L ) | ||||||||
Rm - Tensile strength (MPa) (+A) | 500-720 | |||||||
Rm - Tensile strength (MPa) (+AT) | 490-690 | |||||||
Rp0.2 0.2% proof strength (MPa) (+A) | 200-240 | |||||||
Rp0.2 0.2% proof strength (MPa) (+AT) | 220 | |||||||
KV - Impact energy (J) transverse, (+A) | +20° | -196° | ||||||
60 | 60 | |||||||
KV - Impact energy (J) longitud., (+A) | +20° | |||||||
100 | ||||||||
A - Min. elongation at fracture (%) (+A) | 35-40 | |||||||
A - Min. elongation at fracture (%) longitud., (+AT) | 35 | |||||||
Brinell hardness (HB): (+A) | 215 | |||||||
Brinell hardness (HB): (+AT) | 200 |